Relationships between the microstructure and fracture toughness of microalloyed (API 5L X65) steels Zusammenhänge zwischen Mikrostruktur und Bruchzähigkeit von mikrolegierten (API 5L X65)-Stählen


TAŞ Z., Sönmez N.

Praktische Metallographie/Practical Metallography, cilt.42, sa.6, ss.290-303, 2005 (SCI-Expanded, Scopus)

  • Yayın Türü: Makale / Derleme
  • Cilt numarası: 42 Sayı: 6
  • Basım Tarihi: 2005
  • Doi Numarası: 10.3139/147.100265
  • Dergi Adı: Praktische Metallographie/Practical Metallography
  • Derginin Tarandığı İndeksler: Science Citation Index Expanded (SCI-EXPANDED), Scopus
  • Sayfa Sayıları: ss.290-303
  • Yozgat Bozok Üniversitesi Adresli: Evet

Özet

The present article is intended to examine the relationships between the microstructure and the fracture mechanical properties. It uses the J integral concept for a characterization of the properties of fracture mechanics. The microalloyed steels of the X65/API-5L type were used for this purpose. Some of the individual microstructures were characterized qualitatively, others quantitatively, by means of a light microscope (LM) and a scanning electron microscope (SEM). The examinations of the size and distribution of the non-metallic inclusions and precipitates were made by means of a SEM and an LM, in some cases. Tensile tests and notch bend impact tests were performed to determine the mechanical properties. The properties of fracture mechanics were examined on three-point bending test samples at a room temperature. The multi-sample method was employed to determine the crack growth resistance curve. © Carl Hanser Verlag, München.